From: Effects of paraffin external coating on the degradable flower pot made of sludge cake
Flower pot | Thai Std | Canadian Std | ||
---|---|---|---|---|
TEA (mg kg−1) | Lead (Pb) | 9.55 | 400a | 375b |
Nickel (Ni) | 1.29 | 1600a | 150b | |
Copper (Cu) | 10.38 | –a | 150b | |
LT (μg L−1) | Lead (Pb) | 0.88 | 5000c | |
Nickel (Ni) | 0.12 | 20,000c | ||
Copper (Cu) | 0.57 | 25,000c |